The injection barrel is an important part of the injection molding machine. The injection barrel works together with the injection screw to convey, compact, melt, stir and press the plastic. All of this is done by the rotation of the screw within the barrel.
How to make the nitrided Injection barrel?
Barrelize has its own nitriding furnace in-house. The injection barrel will be put into the nitriding furnace with nitrogen under a certain temperature and humidity environment. Barrelize nitrided injection barrel will be put into the furnace for 5 days and nights. After 5 days' deep barrel nitriding, a nitrided layer with relatively high hardness is formed on the surface of the barrel.
What 's the specification of Barrelize nitrided Injection barrel?
The nitrided layer can reach 0.05-0.07mm. The hardness can reach HV950±50or above, equivalent to HRC68~69.
The general advantage of Barrelize nitrided barrel: it can improve corrosion resistance and wear resistance.
Call us now to talk to our team about your specific demand. We have an expert here to listen to your demands and understand what you are looking for.
Product |
Material Base |
Treatment |
Technical Parameter |
Application |
Barrel |
38CrMoAlA |
Nitriding |
tempering hardness :HB260-280 |
Commonly used for acid-free plastics with GF less than 10%, |
Barrel |
38CrMoAlA |
Bimetallic Fe-based alloy |
Alloy thickness: 1.5-2MM |
Commonly used for adding acid plastic with GF less than 30%,PC/PA |
Barrel |
38CrMoAlA |
Bimetallic Ni-based alloy+15% tungsten carbide powder |
Alloy thickness: l.5-2MM, |
Commonly used for adding acid plastic with GF |
Barrel |
38CrMoAlA |
Bimetallic Ni-based alloy+25% tungsten carbide powder |
Alloy thickness: l.5-2MM |
generally used to add aci lastic PEEK/PPS/LCP/flame retardant |